Semi-Process & High Magnetic Flux Density Specification

Type Grade of CSC Spec. Thickness (mm) Density (kg/dm3) Iron Loss max. (W/kg) 1,5 T/50 Hz Magnetic Flux Density min. (T) B50
Semi Process 50CS600 AC 0.50 7.85 6.0 1.73
50NE1 ANC - 7.80 4.0 1.70
50NE1 ANC - 7.75 3.5 1.67
High Magnetic
Flux Density
35CS250H 0.35 7.65 2.5 1.60
35CS300H - 7.65 3.0 1.60
50CS470H 0.50 7.70 4.7 1.62
50CS600H - 7.75 6.0 1.68
Note
  • This density is used in all calculation of the sectional area of test pieces
  • 1,5 T/50 Hz indicates the iron loss when the frequency is 50 Hz and the maximum magnetic flux density is 1.5T (1.5 Wb/m2)
  • B50 indicates the magnetic flux density under the magnetic force 5000 a/m
  • Iron loss of Semi-Process Product were annealed at 750 °C 2hr
  • Density is for reference only, the actual density will vary with the chemical composition of steel grades